Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 13001 | |
| Number of page(s) | 5 | |
| Section | Posters: Process Microstructure Interactions | |
| DOI | https://doi.org/10.1051/matecconf/20141413001 | |
| Published online | 29 August 2014 | |
- E. Kablov Cast blades of gas turbine engines: alloys, technologies, coatings 2nd ed. (2006) [Google Scholar]
- Yu. Bondarenko, A. Echin, V. Surova, A. Narsky Liteynoye proizvodstvo 5, 36–39 (2011) [Google Scholar]
- V. Gerasimov, E. Visik, E. Kolyadov Liteynoye proizvodstvo. 3, 21–23 (2013) [Google Scholar]
- E. Kablov, Yu. Bondarenko, V. Surova Foundry heat-resistant alloys. Kishkin's effect: science and research compilation, 194–205 (2006) [Google Scholar]
- E. Kablov, N. Petrushin, V. Sidorov, I. Demonis Foundry heat-resistant alloys. Kishkin's effect: science and research compilation, 79–97 (2006) [Google Scholar]
- E. Kablov, Yu. Bondarenko, A. Echin, V. Surova Aviation materials and technologies 1, 3–7 (2012) [Google Scholar]
- R. Shalin, I. Svetlov, E. Kachanov, etc. Monocrystals of the nickel heat-resistant alloys (1997) [Google Scholar]
- N. Petrushin, M. Bronfin, E. Kablov, I. Hatsinskaya, E. Chabina, I. Roschin, O. Timofeeva Foundry heat-resistant alloys.0 Kishkin's effect: science and research compilation, 142–154 (2006) [Google Scholar]
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.