Turbine blades production technique equipment built with a glance of high-gradient directional crystallization process nature
FSUE “All Russian Scientific Research Institute of Aviation Materials” (VIAM), 105005, Radio str. 17, Moscow, Russia
Abstract
The influence of the high-gradient directional crystallization on the structural components (the interdendritic distance and porosity) of the superalloys is presented in the Article. The industrial-scale high-gradient plant of UVNS-6 type and some benefits of its use are shown here as well. Some test specimens manufactured on the UVNS-6 are studied with measurement of the interdendritic distance. The temperature gradient is estimated by experimental method.
© Owned by the authors, published by EDP Sciences, 2014
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.