Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 11005 | |
| Number of page(s) | 6 | |
| Section | Posters: Precipitation | |
| DOI | https://doi.org/10.1051/matecconf/20141411005 | |
| Published online | 29 August 2014 | |
- C. T. Liu and D. P. Pope, Intermetallic Compounds. - Structural Appications of Intermetallic Compounds 55 (John Wiley & Sons, Ltd, 2002) [Google Scholar]
- R. C. Reed, The Superalloys: Fundamentals and Applications (Cambridge University Press, 2008) [Google Scholar]
- B. Reppich, Acta Metall. 30, 87 (1982) [CrossRef] [Google Scholar]
- B. Reppich, P. Schepp, G. Wehner, Acta Metall. 30, 95 (1982) [CrossRef] [Google Scholar]
- G. B. Viswanathan, P. M. Sarosi, M. F. Henry, D. D. Whitis, W. W. Milligan, M. J. Mills, Acta Mater. 53, 3041 (2005) [CrossRef] [Google Scholar]
- T. M. Pollock, A. S. Argon, Acta Metall. Mater. 40, 1 (1992) [Google Scholar]
- L. Kovarik, R. R. Unocic, J. Li, P. Sarosi, C. Shen, Y. Wang, and M. J. Mills, Prog. Mater. Sci. 54, 839 (2009) [CrossRef] [Google Scholar]
- R. C. Reed, N. Matan, D. C. Cox, M. A. Rist, and C. M. F. Rae, Acta Mater. 47, 3367 (1999) [CrossRef] [Google Scholar]
- B. H. Kear, H. G. F. Wilsdorf, Trans. Metall. Soc. AIME. 224, 382 (1962) [Google Scholar]
- E. Nembach, K. Suzuki, M. Ichihara, S. Takeuchi, Philos. Mag. A 51, 607 (1985) [CrossRef] [Google Scholar]
- N. M. Rosengaard, H. L. Skriver, Phys. Rev. B 50, 4848 (1994) [CrossRef] [Google Scholar]
- M. H. Yoo, C. L. Fu, J. A. Horton, Mater. Sci. Eng. A 176, 431 (1994) [CrossRef] [Google Scholar]
- A. F. Voter, S. P. Chen, MRS Proceeding. 82, 175 (1986) [Google Scholar]
- Y. Mishin, Acta Mater. 52, 1451 (2004) [CrossRef] [Google Scholar]
- J. Douin, P. Veyssière, P. Beauchamp, Philos. Mag. A 54, 375 (1986) [Google Scholar]
- T. Kruml, E. Conforto, B. Lo Piccolo, D. Caillard, J. L. Martin, Acta Mater. 50, 5091 (2002) [CrossRef] [Google Scholar]
- H. P. Karnthaler, E. T. Mühlbacher, C. Rentenberger, Acta Mater. 44, 547 (1996) [CrossRef] [Google Scholar]
- D. M. Dimiduk, J. Phys. III 1, 1025 (1991) [Google Scholar]
- A. Korner, Philos. Mag. A 58, 507 (1988) [Google Scholar]
- M. Chandran, S. K. Sondhi, Model. Simul. Mater. Sci. Eng. 19, 025008 (2011) [Google Scholar]
- N. Baluc, H. P. Karnthaler, M. J. Mills, Philos. Mag. A 64, 137 (1991) [CrossRef] [Google Scholar]
- N. Baluc, R. Schäublin, K. J. Hemker, Philos. Mag. Lett. 64, 327 (1991) [CrossRef] [Google Scholar]
- K. V. Vamsi, S. Karthikeyan, Proceeding of Twelfth International Symposium on Superalloys, 521 (The Minerals, Metals and Materials Society (TMS), Warrendale, PA, 2012) [Google Scholar]
- G. Kresse, J. Hafner, Phys. Rev. B 47, 558 (1993) [Google Scholar]
- G. Kresse, J. Furthmüller, Phys. Rev. B 54, 11169 (1996) [NASA ADS] [CrossRef] [Google Scholar]
- G. Kresse, J. Hafner, Phys. Rev. B 49, 14251 (1994) [Google Scholar]
- G. Kresse, J. Furthmüller, Comput. Mater. Sci. 6, 15 (1996) [Google Scholar]
- MedeA version 2.6.6, Materials Design Inc, Angel Fire, NM, USA (2009) [Google Scholar]
- M. Methfessel, A. T. Paxton, Phys. Rev. B 40, 3616 (1989) [Google Scholar]
- J. P. Perdew, K. Burke, M. Ernzerhof, Phys. Rev. Lett. 77, 3865 (1996) [Google Scholar]
- J. P. Perdew, K. Burke, M. Ernzerhof, Phys. Rev. Lett. 78, 1396 (1997) [Google Scholar]
- V. Vitek, Cryst. Lattice Defects 5, 1 (1974) [Google Scholar]
- K. V. Vamsi, S. Karthikeyan (Unpublished) [Google Scholar]
- P. J. Ferreira, P. Müllner, Acta Mater. 46, 4479 (1998) [CrossRef] [Google Scholar]
- P. J. H. Denteneer, W. van Haeringen, J. Phys. C Solid State Phys. 20, L883 (1987) [CrossRef] [Google Scholar]
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.