Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 06001 | |
| Number of page(s) | 6 | |
| Section | Session 6: Mechanical Behavior II: Single Crystal Alloys | |
| DOI | https://doi.org/10.1051/matecconf/20141406001 | |
| Published online | 29 August 2014 | |
- Hopkins S. Testing, Low-Cycle Thermal Mechanical Fatigue, in: ASTM STP 612. 1976 [Google Scholar]
- Rau C Jr, Gemma A, Leverant G. Thermal-Mechanical Fatigue Crack Propagation in Nickel- and Cobalt-Base Superalloys Under Various Strain-Temperature Cycles, in: ASTM STP 520. 1972 [Google Scholar]
- Hahner P, Rinaldi C, Bicego V, Affeldt E, Brendel T, Andersson H, Beck T, Klingelhoffer H, Kuhn H, Koster A. Int J Fatigue 2008;30:372 [Google Scholar]
- Loveday M, Bicego V, Hahner P, Klingelhoffer H, Kuhn H, Roebuck B. Int J Fatigue 2008;30:382 [CrossRef] [Google Scholar]
- Hasselqvist M, Moverare J. Vol 5 Turbo Expo 2007 2007;1:131 [CrossRef] [Google Scholar]
- Moverare J, Johansson S, Reed RC. Acta Mater 2009;57:2266 [Google Scholar]
- Ezz SS, Pope DP, Paidar V. Acta Metall 1982;30:921 [CrossRef] [Google Scholar]
- Arrell D, Hasselqvist M, Sommer J, Moverare J. On TMF Damage, Degradation Effects, and the Associated Tmin Influence on TMF Test Results in γ/γ' Alloys, in: Superalloys 2004. 2004 [Google Scholar]
- Leidermark D, Moverare J, Johansson S, Simonsson K, Sjöström S. Acta Mater 2010;58:4986 [CrossRef] [Google Scholar]
- Kupkovits R a., Smith DJ, Neu RW. Procedia Eng 2010;2:687 [CrossRef] [Google Scholar]
- Moverare JJ, Segersäll M, Sato A, Johansson S, Reed RC. Thermomechanical Fatigue of Single-Crystal Superalloys: Influence of Composition and Microstructure, in: Superalloys 2012 [Google Scholar]
- Zhang JX, Ro Y, Zhou H, Harada H. Scr Mater 2006;54:655 [CrossRef] [Google Scholar]
- Zhang JX, Harada H, Ro Y, Koizumi Y, Kobayashi T. Acta Mater 2008;56:2975 [Google Scholar]
- Segersäll M, Moverare JJ, Simonsson K, Johansson S. Deformation and Damage Mechanisms During Thermomechanical Fatigue of a Single-Crystal Superalloy in the 〈001〉 and 〈011〉 Directions, in: Superalloys 2012 [Google Scholar]
- Knowles DM, Gunturi S. Mater Sci Eng A 2002;328:223 [CrossRef] [Google Scholar]
- Heredia FE, Pope DP. Acta Metall 1986;34:279 [CrossRef] [Google Scholar]
- Segersäll M, Moverare JJ, Leidermark D, Simonsson K. Metall Mater Trans A 2014; Accepted:10.1007/s11661 [Google Scholar]
- Segersäll M, Moverare JJ, Leidermark D, Johansson S. In- and out-of-phase Thermomechanical Fatigue of a Ni-Based Single-Crystal Superalloy, in: EuroSuperalloys 2014 [Google Scholar]
- Moverare JJ, Johansson S. Mater Sci Eng A 2010;527:553 [CrossRef] [Google Scholar]
- Sato A, Moverare J, Hasselqvist M, Reed RC. Metall Mater Trans A 2012;43:2302 [Google Scholar]
- Kovarik L, Unocic RR, Li J, Mills MJ. JOM 2009;61:42 [CrossRef] [Google Scholar]
- Kovarik L, Unocic RR, Li J, Sarosi P, Shen C, Wang Y, Mills MJ. Prog Mater Sci 2009;54:839 [Google Scholar]
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.