Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 03002 | |
| Number of page(s) | 6 | |
| Section | Session 3: Deformation and Damage Mechanisms II: Fatigue, Oxidation and Crack Propagation | |
| DOI | https://doi.org/10.1051/matecconf/20141403002 | |
| Published online | 29 August 2014 | |
- Direct communications within a ongoing EPSRC-Rolls-Royce Strategic Partnership programme. A manuscript has been submitted to Acta Mater [Google Scholar]
- Viskari L, Hörnqvist M, Moore KL, Cao Y, Stiller K., Acta Mater 2013;61:3630 [CrossRef] [Google Scholar]
- Andrieu E, Molins R, Ghonem H, Pineau A. Mater Sci Eng A 1992;154:21 [Google Scholar]
- Goswami T. Int J Fatigue 1999;21:55 [Google Scholar]
- Wei RP, Miller C, Huang Z, Simmons GW, Harlow DG. Eng Fract Mech 2009;76:715 [CrossRef] [Google Scholar]
- Pfaendtner JA, McMahon Jr CJ. Acta Mater 2001;49:3369 [Google Scholar]
- Bika D, McMahon Jr CJ. Acta Metall Mater 1995;43:1909 [CrossRef] [Google Scholar]
- Krupp U, McMahon Jr CJ. J Alloys Compd 2004;378:79 [CrossRef] [Google Scholar]
- Ma L, Chang K-M. Scr Mater 2003;48:1271 [CrossRef] [Google Scholar]
- Viskari L, Cao Y, Norell M, Sjöberg G, Stiller K. Mater Sci Eng A 2011;528:2570 [CrossRef] [Google Scholar]
- Kitaguchi HS, Li HY, Evans HE, Ding RG, Jones IP, Baxter G, Bowen P. Acta Mater 2013;61:1968 [CrossRef] [Google Scholar]
- Miller CF, Simmons GW, Wei RP. Scr Mater 2001;44:2405 [Google Scholar]
- Wilkinson AJ, Hirsch PB. Micron 1997;28:279 [CrossRef] [Google Scholar]
- Krupp U, Kane WM, Liu X, Dueber O, Laird C, McMahon Jr CJ. Mater Sci Eng A 2003;349:213 [CrossRef] [Google Scholar]
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.