Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 16002 | |
| Number of page(s) | 6 | |
| Section | Posters: Deformation and Damage Mechanisms II: Fatigue, Oxidation, Crack Propagation | |
| DOI | https://doi.org/10.1051/matecconf/20141416002 | |
| Published online | 29 August 2014 | |
- L.M. Pike, Proceedings of Superalloys 2008, TMS, 191 (2008) [Google Scholar]
- L.M. Pike, Proceedings of ASME Turbo Expo 2006, ASME, GT2006-91204 (2006) [Google Scholar]
- P.G. McCormick, Acta Metall. 20, 351 (1972) [CrossRef] [Google Scholar]
- R.W. Hayes, W. C. Hayes, Acta Metall. 30, 1295 (1982) [CrossRef] [Google Scholar]
- K. Gopinath, A.K. Gogia, S.V. Kamat, U. Ramamurty, Acta Mater. 57, 1243 (2009) [CrossRef] [Google Scholar]
- C.L. Hale, W.S. Rollings, M.L. Weaver, Mat. Sci. Eng. A 300, 153 (2001) [CrossRef] [Google Scholar]
- A. Nagesha, S. Goyal, M. Nandagopal, P. Parameswaran, R. Sandhya, M.D. Mathew, S.K. Mannan, Mat. Sci. Eng. A 546, 34 (2012) [CrossRef] [Google Scholar]
- S.A. Nalawade, M. Sundararaman, R. Kishore, J.G. Shah, Scripta Mater. 59, 991 (2008) [CrossRef] [Google Scholar]
- W. Chen, M.C. Chaturvedi, Mat. Sci. Eng. A 229, 163 (1997) [CrossRef] [Google Scholar]
- P. Rodriguez, Bull. Mater. Sci. 6, 653 (1984) [CrossRef] [Google Scholar]
- S.L. Mannan, Bull. Mater. Sci. 6, 561, (1993) [CrossRef] [Google Scholar]
- B.A. Lerch, N. Jayaraman, S.D. Antolovich, Mat. Sci. Eng. 66, 151 (1984) [CrossRef] [Google Scholar]
- K. Gopinath, A.K. Gogia, S.V. Kamat, R. Balamuralikrishnan, U. Ramamurty, Acta Mater. 57, 3450 (2009) [CrossRef] [Google Scholar]
- R.E. Stoltz, A.G. Pineau, Mat. Sci. Eng. 34, 275 (1978) [CrossRef] [Google Scholar]
- B. Lerch, V. Gerold, Acta Metall. 33, 1709 (1985) [CrossRef] [Google Scholar]
- M. Sundararaman, W. Chen, V. Singh, R.P. Wahi, Acta Metall. Mater. 38, 1813 (1990) [CrossRef] [Google Scholar]
- E. Pink, A. Grinberg, Acta Metall. 30, 2135 (1982) [CrossRef] [Google Scholar]
- Gale WF, Totemeier TC, editors. Smithells metals reference book. London: Butterworth-Heinemann; 2004. p. 3–25 [Google Scholar]
- Y. Nakada, A. S. Keh, Acta Metall. 18, 437 (1970) [CrossRef] [Google Scholar]
- K. Bhanu Sankara Rao, S. Kalluri, G.R. Halford, M.A. McGaw, Scripta Metall. Mater. 32, 493 (1995) [CrossRef] [Google Scholar]
- J. Cermák, H. Mehrer, Acta Metall. Mater. 42, 1345 (1994) [CrossRef] [Google Scholar]
- R.W. Balluffi, phys. stat. sol. 42, 11 (1970) [CrossRef] [Google Scholar]
- J. Cermák, Mat. Sci. Eng. A 148, 279 (1991) [CrossRef] [Google Scholar]
- V. Shankar, M. Valsan, K. Bhanu Sankara Rao, S.L. Mannan, Metall. Mater. Trans. A 35A, 3129 (2004) [CrossRef] [Google Scholar]
- M. Clavel, A. Pineau, Mat. Sci. Eng. 55, 157 (1982) [Google Scholar]
- M. Valsan, D.H. Sastry, K. Bhanu Sankara Rao, S.L. Mannan, Metall. Mater. Trans. A 25A, 159 (1994) [CrossRef] [Google Scholar]
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.