Issue |
MATEC Web Conf.
Volume 403, 2024
SUBLime Conference 2024 – Towards the Next Generation of Sustainable Masonry Systems: Mortars, Renders, Plasters and Other Challenges
|
|
---|---|---|
Article Number | 07007 | |
Number of page(s) | 17 | |
Section | Conservation, Repair and Strengthening | |
DOI | https://doi.org/10.1051/matecconf/202440307007 | |
Published online | 16 September 2024 |
Characterization of the degradation rate of ceramic-tiled facades
1 Universidade de Brasília/UnB, Programa de Pós-graduação em Estruturas e Construção Civil, Brasília, DF, 70910-900, Brazil
2 Universidade de Brasília/UnB, Programa de Pós-graduação em Estruturas e Construção Civil, Brasília, DF, 70910-900, Brazil
Facades are systems fixed externally to the building that perform the function of protecting the internal environment, thermal comfort and control lighting. The degradation of facades occurs due to the action of agents and mechanisms that are capable of causing alterations in the chemical and physical characteristics of materials. It depends on factors such as orientation, degree of exposure to agents and construction processes. Because the facades have different exposure conditions, degradation manifests itself heterogeneously. Given the need to understand the evolutionary behavior of degradation, we propose to characterize degradation based on its velocity as a function of increasing age of buildings. This new index helps in the study of degradation, since unlike the FGD (general degradation factor), it considers the age factor of the sample. This research was applied in 306 samples of facades located in Brasilia, Brazil. Degradation is quantified by the degradation measurement method (DMM). The speed of the degradation consists of quantifying the degradation of each sample over a year. For the quantification of the speed, three characteristic intervals are adopted (low, medium and high speed). It is observed that, with higher values, degradation becomes widespread. For the high degradation rate, more than half of the samples have a northern orientation. The high percentage of samples with a northern orientation and a high degradation rate shows that this orientation has a higher criticality of degradation.
© The Authors, published by EDP Sciences, 2024
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.