EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 17004 | |
| Number of page(s) | 5 | |
| Section | Posters: Alloy Development I: Ni Based Alloys | |
| DOI | https://doi.org/10.1051/matecconf/20141417004 | |
| Published online | 29 August 2014 | |
HAYNES 244 alloy – a new 760 ∘C capable low thermal expansion alloy
Haynes International, Inc., Research and Technology Department, Kokomo, Indiana 46904-9013, USA
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
HAYNES® 244TM alloy is a new 760∘C capable, high strength low thermal expansion (CTE) alloy. Its nominal chemical composition in weight percent is Ni – 8 Cr – 22.5 Mo – 6 W. Recently, a first mill-scale heat of 244 alloy was melted by Haynes International, and processed to various product forms such as re-forge billet, plate, and sheet. This paper presents key attributes of this new alloy (CTE, strength, low-cycle fatigue performance, oxidation resistance, thermal stability) as they pertain to the intended use in rings and seals of advanced gas turbines.
© Owned by the authors, published by EDP Sciences, 2014
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.