Large scale 3-D phase-field simulation of coarsening in Ni-base superalloys
Interdisciplinary Centre for Advanced Materials Simulation (ICAMS), Ruhr University Bochum, Germany
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
In this study we present a large scale numerical simulation of γ-γ′ microstructure evolution in Ni-base superalloy using the multi-phase field method in three dimensions. We numerically simulated precipitation hardening heat treatment cycles. Large scale three dimensional simulations are necessary in order to get sufficient statistics for predicting the morphological evolution, average γ′ precipitate size, precipitates size distribution over time and ripening exponent for a given temperature and composition. A detailed analysis of obtained result is presented emphasising the effect of elastic interaction on the coarsening kinetics in Ni-base superalloy. The study is performed using the phase-field modelling library “OpenPhase” which is based on a multi-phase field multi-component model.
Note to the reader concerning this PDF file: legends of the figures 6 and 7 were added on October 1st, 2014.
© Owned by the authors, published by EDP Sciences, 2014
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.