Probing the strain distribution within a single crystal superalloy during high temperature testing
1 Institut Jean Lamour (UMR CNRS-UL N ∘ 7198), Labex DAMAS, Parc de Saurupt, 54000 Nancy, France
2 LiPhy, 140 Avenue de la Physique, BP. 87, 38402 Saint-Martin-d'Hères, France
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
The combination of in situ high resolution diffraction experiments with synchrotron radiation and mechanical and diffraction modelling is used to investigate the microstructure and mechanical state of single crystal superalloys during high temperature tests: a very high temperature annealing without external load and a creep test.
© Owned by the authors, published by EDP Sciences, 2014
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.