Study on the effect of pre-treatment of Oil Palm Shell (OPS) as coarse aggregate using hot water 50-°C and room temperature water 28-°C to lightweight concrete strength
MATEC Web Conf., 276 (2019) 01023
Published online: 15 March 2019
DOI: 10.1051/matecconf/201927601023