  1. P.J. Sánchez-Soto, M.A. Avilés, J.C. del Río, J.M. Ginés, J. Pascual, J.L. Pérez-Rodríguez, Thermal study of the effect of several solvents on polymerization of acrylonitrile and their subsequent pyrolysis, J. Anal. Appl. Pyrolysis 59, 155–172 (2001). [CrossRef]
  2. X. Huang, Fabrication and properties of carbon fibers, Materials 2, 2369–2403 (2009). [CrossRef]
  3. T.-H. Ko, S.-C. Liau, M.-F. Lin, Preparation of graphite fibres from a modified PAN precursor, J. Mater. Sci. 27, 6071–6078 (1992). [CrossRef]
  4. L. Jie, Z. Wangxi, Structural changes during the thermal stabilization of modified and original polyacrylonitrile precursors, J. Appl. Polym. Sci. 97, 2047–2053 (2005). [CrossRef]
  5. R.B. Mathur, O.P. Bahl, J. Mittal, Advances in the development of high performance carbon fibers from PAN precursor, Compos. Sci. Technol. 51,223–230 (1994). [CrossRef]
  6. J. Mittal, R.B. Mathur, O.P. Bahl, Post spinning modification of PAN fibres—a review, Carbon 35, 1713–1722 (1997). [CrossRef]
  7. X. Huang, Fabrication and properties of carbon fibers, Materials 2, 2369–2403 (2009). [CrossRef]
  8. Yusof, N. & Ismail, A., Post spinning and pyrolysis processes of polyacrylonitrile (PAN)-based carbon fiber and activated carbon fiber: A review, Journal of Analytical and Applied Pyrolysis 93, 1 – 13 (2012) [CrossRef]
  9. Mittal, J.; Mathur, R.; Bahl, O. & Inagaki, M. Post spinning treatment of PAN fibers using succinic acid to produce high performance carbon fibers, Carbon, 36, 893 – 897 (1998) [CrossRef]
  10. Gupta, A. & Harrison, I. New aspects in the oxidative stabilization of PAN-based carbon fibers: II, Carbon, 35, 809 – 818 (1997) [CrossRef]